Products

Radilon® S LRV300ER 339 E NER

Radilon® S LRV300ER 339 E NER

Manufacturer: RADICI
Produced At:
 Europe / China
Product Category: Polyamide 6 (Nylon 6)
Product No: Radilon S LRV300ER 339 E NER 
Product Quantity: 25KG / BAG
Product Features: Good Flow,Good Surface Finish,High Stiffness

Radilon® S LRV300ER 339 E NER

Polyamide 6
Product Description:

PA6 30% glass fiber reinforced injection moulding grade. High flowability. Deep black colour.

Suitable for parts requiring high stiffness and good mechanical resistance. Good surface aspect and easier flow.

ISO 1043 : PA6 GF30


Filler / Reinforcement 
  • Glass Fiber, 30% Filler by Weight

Features 
  • Good Flow,Good Surface Finish,High Stiffness
RoHS Compliance 
  • RoHS Compliant

Appearance 
  • Black

Processing Method 
  • Injection Molding

Resin ID (ISO 1043)
  • PA6 GF30

Physical
Dry
Conditioned
Unit
Test Method
Density
1.35
--
g/cm³
ISO 1183
Water Absorption



ISO 62
Saturation, 73°F, 0.0787 in
7.5
--
%

Equilibrium, 73°F, 0.0787 in, 50% RH
2.0
--
%

Mechanical
Dry
Conditioned
Unit
Test Method
Tensile Modulus
1.44E+6
928000
psi
ISO 527-2/1A/1
Tensile Stress (Break)
23900
15200
psi
ISO 527-2/1A/5
Tensile Strain (Break)
3.0
4.0
%
ISO 527-2/1A/5
Flexural Modulus 2
1.26E+6
--
psi
ISO 178
Flexural Stress 2
35500
--
psi
ISO 178
Impact
Dry
Conditioned
Unit
Test Method
Charpy Notched Impact Strength



ISO 179/1eA
-22°F
4.0
--
ft·lb/in²

73°F
4.5
8.6
ft·lb/in²

Charpy Unnotched Impact Strength



ISO 179/1eU
-22°F
24
--
ft·lb/in²

73°F
31
38
ft·lb/in²

Thermal
Dry
Conditioned
Unit
Test Method
Heat Deflection Temperature (264 psi, Unannealed)
392
--
°F
ISO 75-2/Af
Vicat Softening Temperature
410
--
°F
ISO 306/B50
Melting Temperature 3
428
--
°F
ISO 11357
Electrical
Dry
Conditioned
Unit
Test Method
Surface Resistivity
1.0E+12
1.0E+10
ohms
IEC 60093
Volume Resistivity
1.0E+15
1.0E+13
ohms·cm
IEC 60093
Comparative Tracking Index
550
--
V
IEC 60112
Flammability
Dry
Conditioned
Unit
Test Method
Burning Rate
0.0
--
in/min
FMVSS 302
Flame Rating (0.031 in)
HB
--

UL 94
Glow Wire Flammability Index (0.08 in)
1290
--
°F
IEC 60695-2-12
Injection
Dry
Unit

Drying Temperature - Desiccant Dryer
176
°F

Drying Time - Desiccant Dryer
2.0 to 4.0
hr

Dew Point - Desiccant Dryer
< -4
°F

Suggested Max Moisture
0.15
%

Processing (Melt) Temp
464 to 536
°F

Mold Temperature
176 to 194
°F

Injection Rate
Moderate-Fast




Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields