Products

Akulon® S-KVS

Akulon® S-KVS

Manufacturer: Envalior/DSM
Produced At: Europe / China
Product Category: Nylon 66(PA66)
Product No: Akulon® S-KVS 
Product Quantity: 25KG / BAG
Product Features: Flame Retardant

Akulon® S-KVS

Polyamide 66

Product Description:
Flame Retardant

Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Additive 
  • Flame Retardant

Features 
  • Flame Retardant

Processing Method 
  • Injection Molding

Physical
Nominal Value
Unit
Test Method
Density
1.34
g/cm³
ISO 1183
Mechanical
Nominal Value
Unit
Test Method
Tensile Modulus
522000
psi
ISO 527-2
Tensile Stress (Break)
11600
psi
ISO 527-2
Tensile Strain


ISO 527-2
Yield
4.3
%

Break
11
%

Flexural Modulus
479000
psi
ISO 178
Flexural Stress
15200
psi
ISO 178
Impact
Nominal Value
Unit
Test Method
Charpy Notched Impact Strength (73°F)
1.7
ft·lb/in²
ISO 179/1eA
Charpy Unnotched Impact Strength (73°F)
42
ft·lb/in²
ISO 179/1eU
Notched Izod Impact Strength (73°F)
2.2
ft·lb/in²
ISO 180/1A
Electrical
Nominal Value
Unit
Test Method
Comparative Tracking Index
250
V
IEC 60112
Flammability
Nominal Value
Unit
Test Method
Flammability Classification


IEC 60695-11-10, -20
0.016 in
V-0


0.12 in
V-0


Glow Wire Flammability Index


IEC 60695-2-12
0.016 in
1760
°F

0.12 in
1760
°F

Glow Wire Ignition Temperature


IEC 60695-2-13
0.016 in
1760
°F

0.12 in
1470
°F

Injection
Nominal Value
Unit

Drying Temperature
176
°F

Drying Time
2.0 to 4.0
hr

Rear Temperature
482 to 500
°F

Middle Temperature
500 to 518
°F

Front Temperature
509 to 527
°F

Nozzle Temperature
500 to 509
°F

Processing (Melt) Temp
509 to 527
°F

Mold Temperature
122 to 176
°F

Injection Rate
Moderate-Fast


Back Pressure
435 to 1450
psi

Screw Compression Ratio
2.5:1.0




Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields